▶ Try the interactive furnace in your browser
Python models of the core steps in a silicon fab: thermal oxidation, dopant predeposition and drive-in, ion implantation, sheet resistance and oxide colour. Each model is validated against published data or an exact analytic solution (32 automated tests run on every commit).
The colour of an oxidised wafer, computed from thin-film interference optics and CIE colour science, with no lookup table. It reproduces the standard thermal-oxide colour chart (Pliskin & Conrad) to within ~10 nm, e.g. royal blue at 120 nm, gold at 210 nm, red-violet at 270 nm.
Run a wafer through a process traveler and get the resulting doping profile, junction depth, sheet resistance and oxide thickness, the same numbers a fab would measure with a four-point probe, ellipsometer and SIMS.
from fabsim import Wafer w = Wafer(substrate="n", background=1e15) # n-type <100> wafer, 1e15 cm^-3 w.oxidize(1000, 90, ambient="wet").strip_oxide() # sacrificial oxide, HF strip w.predeposit("B", 950, 30, surface_conc=1e20) # boron predeposition w.oxidize(1100, 60, ambient="dry") # drive-in under a growing oxide print(w.report())
Oxide thickness: 111 nm (#637dba)
Junction depth: 1.355 um
Sheet resistance: 239.4 ohm/sq
Surface doping: 7.38e+18 cm^-3 (p-type)
Every step diffuses all dopants already in the wafer at that step's temperature, so later high-temperature steps move earlier junctions, as they do in a real flow. Oxidation consumes 0.44 µm of Si per µm of oxide grown.
| Step | Model | Validation (see tests/) |
|---|---|---|
| Thermal oxidation | Deal-Grove linear-parabolic, dry & wet, <100>/<111> | Rate constants within 25 % of Deal & Grove's (1965) measured tables, 800–1200 °C; linear and parabolic limits; split steps equal one long step |
| Predeposition | Fick's 2nd law, numerical (Crank-Nicolson) with fixed surface concentration | Matches the analytic erfc solution to < 0.2 % of Cs |
| Drive-in / anneal | Same solver, zero-flux surface | Matches the analytic half-Gaussian to < 1 %; dose conserved to 0.1 % |
| Ion implantation | Gaussian with Rp, ΔRp from LSS range tables | Dose integrates exactly; peak at Rp; As < P < B range ordering |
| Mobility / resistivity | Caughey-Thomas, 300 K | Within 20 % of the Irvin curves for n and p, 1015–1018 cm-3 |
| Sheet resistance | Rs = 1 / (q∫μ(N)|Nnet|dx), four-point probe factor π/ln2 | Uniform layer reduces exactly to ρ/t |
| Oxide colour | Airy thin-film reflectance → CIE 1931 XYZ → sRGB | Bare Si reflects 35 %; quarter-wave minimum at λ/4n; hues match the standard colour chart |
- Diffusivities are intrinsic: no concentration-dependent, oxidation-enhanced or transient-enhanced diffusion, so heavily doped profiles diffuse too little.
- No dopant segregation at the Si/SiO2 interface (in reality boron is pulled into a growing oxide and phosphorus piles up beneath it).
- Implants are single Gaussians (no channelling tails or Pearson-IV skew) and the oxide is treated as transparent to ions.
- 1-D only: no lateral diffusion under mask edges.
- Dry-oxidation thin-film regime handled with Deal & Grove's 25 nm effective-initial-oxide convention.
pip install -e ".[dev]" pytest -v # 32 validation tests python examples/make_figures.py # regenerate figures/
The browser version (in docs/) re-implements the oxidation,
colour and diffusion models in plain JavaScript, so it runs with no install.
- B. E. Deal & A. S. Grove, J. Appl. Phys. 36, 3770 (1965): oxidation kinetics
- R. B. Fair, in Impurity Doping Processes in Silicon (1981): intrinsic diffusivities
- J. F. Gibbons, W. S. Johnson & S. W. Mylroie, Projected Range Statistics (1975): implant ranges
- D. M. Caughey & R. E. Thomas, Proc. IEEE 55, 2192 (1967): mobility model
- I. H. Malitson, JOSA 55, 1205 (1965); D. E. Aspnes & A. A. Studna, PRB 27, 985 (1983): optical constants
- C. Wyman, P.-P. Sloan & P. Shirley, JCGT 2(2) (2013): analytic CIE colour-matching functions
- W. A. Pliskin & E. E. Conrad, IBM J. Res. Dev. 8, 43 (1964): oxide colour chart
- R. C. Jaeger, Introduction to Microelectronic Fabrication; J. D. Plummer et al., Silicon VLSI Technology
Daniel Shaheen · Electrical Engineering (Micro & Nano Devices), Texas State University · MIT License